उत्पत्ति के प्लेस
Guangdong, China
आवेदन
high thermal conductivity
Hardness
35±10 / 25±10 Shore C
Thermal resistance
≤0.06 / ≤0.01
Volume Resistivity
>1.0*10^12 Ω.cm
Breakdown Voltage
≥6 KV/mm
Thermal conductivity (±0.3)
3.8W/mk, 8.0W/mk
Temperature Range
-40~+160 ℃
Flame retardant performance
V-0